Astm C642 Density Absorption Voids In Hardened Concrete -
So, the technician brings out the hot plate. The sample is boiled in distilled water for . Boiling reduces the surface tension of the water and expands the air in the pores, driving it out. After boiling, the sample cools overnight while still submerged.
Armed with ASTM C642 data, the owner rejected the deck. The contractor demolished and repoured. The test cost less than $500 per core. The replacement cost $2.3 million. Concrete is not a rock. It is a manufactured geology, and its performance depends entirely on the geometry of its emptiness. ASTM C642 is not glamorous. It involves no high-speed cameras or finite element models. It is just a scale, an oven, a boiling pot, and a calculator. astm c642 density absorption voids in hardened concrete
Note: Values >20% permeable voids generally indicate poor-quality concrete or a mix design error. So, the technician brings out the hot plate
| Property | Typical Value | | :--- | :--- | | Dry Density | 125 – 155 lb/ft³ (2000 – 2480 kg/m³) | | Absorption | 4 – 8% | | Permeable Voids | 12 – 18% | After boiling, the sample cools overnight while still
The bridge had stood for only seven winters. On paper, its mix design was perfect: a water-to-cement ratio of 0.45, an air-entrainment target of 6%, and a specified compressive strength of 4,500 psi. Yet, the underside of the deck looked like a topographic map of the moon—scaled, spalled, and weeping rust stains.
[ D_dry = [A / (B-C)] \times \rho_water ] What it means: The mass of solid concrete per unit volume, including pores. A low dry density might indicate lightweight aggregate or excessive voids.